Main Causes of Post‑Cooling Warping

Warping roots in internal stress, caused by uneven material shrinkage during cooling.

  • Unbalanced cooling: Uneven cooling on two sides creates temperature difference, resulting in different shrinkage rates.
  • Unstable extrusion: Improper barrel / die temperature, mismatched screw‑feeding speed leads to inconsistent melt flow.
  • Improper traction: Excess or fluctuating haul‑off speed produces tensile stress, releasing as deformation after cooling.
  • Raw material & formula: Mixed PP of different melt indexes, excessive filler or poor‑quality recycled PP aggravates shrinkage deviation.
  • Uneven die gap: Inconsistent die clearance causes uneven output and local thickness difference.

Quick Adjustment Reference

Problem Adjustment Solution
Single‑side warping Balance cooling water flow of calibration tank
Overall board bending Stabilize extrusion temperature, avoid sharp changes
Traction‑related deformation Maintain constant haul‑off speed, avoid over‑pulling
Twist from thickness difference Recalibrate die gap for uniform melt outflow

Practical Production Fixes

  • Balance cooling system: Keep equal water flow and temperature on both sides. Apply gradual cooling instead of rapid quenching to cut internal stress.
  • Stabilize extrusion parameters: Hold steady barrel and die temperature. Match screw and feeding speed for homogeneous melt.
  • Optimize traction: Keep constant haul‑off speed; do not pursue high output by speeding up blindly.
  • Maintain die regularly: Check die gap and remove carbon deposits. Worn dies will keep producing warped boards.
  • Improve formula: Avoid blending PP with big melt‑index gaps. Optimize filler dispersion for filled or recycled PP.

Conclusion

PP hollow board post‑cooling warping comes from unbalanced cooling, unstable extrusion, improper traction and die issues. Troubleshoot step‑by‑step from cooling tank, extruder, die and raw materials. Reducing residual internal stress improves finished‑product yield.

Hot Tags: pe/pp/pc hollow sheet/plate/board sheet extrusion production line, China pe/pp/pc hollow sheet/plate/board sheet extrusion production line manufacturers, suppliers, factory, PC Hollow Sheet Production Line, PP Hollow Sheet Extrusion Line, XPS Foam Board Production Line, plastic sheet extrusion line, PC Transparent Sheet Production Line, PE Thick Sheet Production Line